Structure and magnetic properties of bulk nanocrystalline Dy metal prepared by spark plasma sintering
Rent:
Rent this article for
USD
10.1063/1.3003863
/content/aip/journal/apl/93/20/10.1063/1.3003863
http://aip.metastore.ingenta.com/content/aip/journal/apl/93/20/10.1063/1.3003863
View: Figures

Figures

Image of FIG. 1.
FIG. 1.

TEM images of bulk nanocrystalline Dy metals prepared by SPS: (a) sintered at , (b) sintered at . Insets: the corresponding SAED patterns of the crystal grains and indexing.

Image of FIG. 2.
FIG. 2.

XRD patterns of bulk Dy metals: curve A is the sample sintered at , curve B is the sample sintered at , and curve C is the coarse-grained sample.

Image of FIG. 3.
FIG. 3.

Temperature dependence of the dc magnetization (field cooling mode) of the bulk Dy samples under external magnetic field: curve A is the sample sintered at , curve B is the sample sintered at , and curve C is the coarse-grained sample. Inset: magnetization curves of the sintered sample upon cooling and heating processes.

Image of FIG. 4.
FIG. 4.

Magnetization curves of the bulk Dy samples: curve A is the sample sintered at , curve B is the sample sintered at , and curve C is the coarse-grained sample. Inset: the coercive force of the three samples at .

Loading

Article metrics loading...

/content/aip/journal/apl/93/20/10.1063/1.3003863
2008-11-17
2014-04-18
Loading

Full text loading...

This is a required field
Please enter a valid email address
752b84549af89a08dbdd7fdb8b9568b5 journal.articlezxybnytfddd
Scitation: Structure and magnetic properties of bulk nanocrystalline Dy metal prepared by spark plasma sintering
http://aip.metastore.ingenta.com/content/aip/journal/apl/93/20/10.1063/1.3003863
10.1063/1.3003863
SEARCH_EXPAND_ITEM